(1).Twin-bangon polycarbonate takardar kauri: 4mm, 6mm, 8mm, 10mm, 12mm, da dai sauransu
(2).Triple-banuwar polycarbonate takardar kauri: 8mm, 10mm, 12mm, 14mm, 16mm, 18mm, 20mm, da dai sauransu
(3).Hudu-bangon polycarbonate takardar kauri: 6mm, 8mm, 10mm, 12mm, 16mm, 20mm, da dai sauransu
(4).Biyar-bangon polycarbonate takardar kauri: 8mm, 10mm, 12mm, da dai sauransu
(5).Six-bangon polycarbonate takardar kauri: 16mm, 20mm, 25mm, da dai sauransu
(6).X-Profile polycarbonate takardar kauri: 10mm, 12mm, 14mm, 16mm, 18mm, 20mm, da dai sauransu
(7).Kauri polycarbonate na saƙar zuma: 6mm, 8mm, 10mm, 12mm, da dai sauransu.
Nisa: 1220mm, 2100mm
Length: Babu iyaka (Shawarar 5800mm, 6000mm, 11800mm, 12000mm don dacewa da ganga 20' & 40' ganga)
Launi: bayyananne / m, tafkin blue, kore, blue, opal, fari, launin ruwan kasa / tagulla, silvery launin toka, ja, rawaya, da dai sauransu.
Bayanan Fasaha (Twin bango polycarbonate hollow sheet) | ||
Halaye | Naúrar | Bayanai |
Ƙarfin tasiri | J/m | 2.1 |
watsa haske | % | 50-85 |
Ƙayyade Ƙaƙƙarfan nauyi | g/m | 1.2 |
Ƙaddamarwar thermal faɗaɗa | mm/m ℃ | 0.065 |
Yanayin sabis | ℃ | -40 ℃ ~ + 120 ℃ |
Zafi conductively | W/m²℃ | 3.0-5.0 |
Ƙarfin sassauƙa | N/mm² | 100 |
Modulus na elasticity | Mpa | 2400 |
Tasirin rufin sauti | db | 20 decibel rage don 10mm pc sheet |
Ƙarfin ƙarfi | N/mm² | ≥60 |
Gwaji Data
Fiberglas | Taishan E-Glass | Anti-UV | ≥99% |
Nauyi | 1.4kg/m2/mm | Haƙuri na Zazzabi | -20ºC zuwa 80ºC |
Matsayin Samfura | GB/T-14206 | Ƙarfin Shear | 92 MPa |
Ƙarfin Ƙarfin Ƙarfi | 75 MPa | Ƙarfin Flexural | 110 MPa |
Thermal Conductivity | 0.158 W/M·K | Thermal Expansion Coefficient | 2.55x10-5 cm/cm/ºC |
Launin samfur
Abubuwan Samfur
1. Kyakkyawan watsa haske, har zuwa 18% -80%
2. Polycarbonate shine filastik injiniyan injiniya mafi jurewa, wanda shine sau 10-27 sama da gilashin plexigous kuma ba zai juya rawaya a rana ba.
3. A saman yana da 50 micron anti-ultraviolet shafi, shekaru 10 na ingancin tabbacin, ba zai haifar da yellowing
4. Zazzabi tsakanin -40 ℃ da +120 ℃ ba zai haifar da nakasawa da sauran ingancin lalacewa ba.
5. Hasken nauyi, mai sauƙin ɗauka da shigarwa
Zane Samfura Mai Ma'ana
Na'urorin haɗi